Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 30-130 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 9 % Show Supplier Material materials with Dehnung of 9 % | min. |
Streckgrenze | 700.0 MPa Show Supplier Material materials with Streckgrenze of 700.0 MPa | min., RP02 |
Zugfestigkeit | 800.0 - 1400.0 MPa Show Supplier Material materials with Zugfestigkeit of 800.0 - 1400.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 1.3 - 1.7 % Show Supplier Material materials with Chrom of 1.3 - 1.7 % | |
Kohlenstoff | 0.3 - 0.38 % Show Supplier Material materials with Kohlenstoff of 0.3 - 0.38 % | |
Mangan | 0.5 - 0.8 % Show Supplier Material materials with Mangan of 0.5 - 0.8 % | |
Molybdän | 0.15 - 0.3 % Show Supplier Material materials with Molybdän of 0.15 - 0.3 % | |
Nickel | 1.3 - 1.7 % Show Supplier Material materials with Nickel of 1.3 - 1.7 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % | |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Tool technology, Automotive engineering | |
Processing history | Quenched and Tempered and Forged |