Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-120mm - Hexagonal Bar: 13- 24 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 10 % Show Supplier Material materials with Dehnung of 10 % | min. |
Streckgrenze | 500.0 MPa Show Supplier Material materials with Streckgrenze of 500.0 MPa | min., RP02 |
Zugfestigkeit | 650.0 - 1200.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 1200.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % | |
Kohlenstoff | 0.38 - 0.45 % Show Supplier Material materials with Kohlenstoff of 0.38 - 0.45 % | |
Mangan | 0.6 - 0.99 % Show Supplier Material materials with Mangan of 0.6 - 0.99 % | |
Molybdän | 0.15 - 0.3 % Show Supplier Material materials with Molybdän of 0.15 - 0.3 % | |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.02 - 0.035 % Show Supplier Material materials with Schwefel of 0.02 - 0.035 % | |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, Mechanical Engineering, Automotive engineering | |
Processing history | Quenched and Tempered and Cold-drawn |