Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 10.68-75.75 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 16 % Show Supplier Material materials with Dehnung of 16 % | min. |
Streckgrenze | 550.0 MPa Show Supplier Material materials with Streckgrenze of 550.0 MPa | min., RP02 |
Zugfestigkeit | 700.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 700.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 1.2 - 1.5 % Show Supplier Material materials with Chrom of 1.2 - 1.5 % | |
Kohlenstoff | 0.17 - 0.25 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.25 % | |
Mangan | 0.4 - 0.8 % Show Supplier Material materials with Mangan of 0.4 - 0.8 % | |
Molybdän | 0.55 - 0.8 % Show Supplier Material materials with Molybdän of 0.55 - 0.8 % | |
Nickel | 0.6 % Show Supplier Material materials with Nickel of 0.6 % | max. |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. |
Vanadium | 0.2 - 0.35 % Show Supplier Material materials with Vanadium of 0.2 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Connecting parts | |
Processing history | Quenched and Tempered and Pealed |