Abmessung
Property | Value |
---|---|
Dimensions | Round-Bar length: 25-170 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 11 % Show Supplier Material materials with Dehnung of 11 % | min. |
Streckgrenze | 800.0 MPa Show Supplier Material materials with Streckgrenze of 800.0 MPa | min., RP02 |
Zugfestigkeit | 1250.0 - 1450.0 MPa Show Supplier Material materials with Zugfestigkeit of 1250.0 - 1450.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.015 % Show Supplier Material materials with Aluminium of 0.015 % | max. |
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % | |
Kohlenstoff | 0.36 - 0.44 % Show Supplier Material materials with Kohlenstoff of 0.36 - 0.44 % | |
Mangan | 0.35 - 0.85 % Show Supplier Material materials with Mangan of 0.35 - 0.85 % | |
Molybdän | 0.6 - 0.75 % Show Supplier Material materials with Molybdän of 0.6 - 0.75 % | |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % | |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % | |
Vanadium | 0.25 - 0.35 % Show Supplier Material materials with Vanadium of 0.25 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Engineering, Apparatus engineering, Connecting parts | |
Processing history | Quenched and Tempered and Forged |