EPDM/PP Deprene 101-64

Alternative and trade names
Deprene 101-64
Want to keep this datasheet? Save it now in your required format

Description

Deprene is vulcanized EPDM/PP thermoplastic elastomer, as well as Santoprene and Sarlink. With advantage of thermoplastic process, Coloration, recycle etc., Deprene is the ideal material to replace EPDM, NBR and PVC.

This material data has been provided by Lingen Plastic Rubber Co..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Supplier Material materials with Density of 0.95 g/cm³

ASTM D297

Mechanical

PropertyTemperatureValueComment

Compression set

23.0 °C

18 [-]

Show Supplier Material materials with Compression set of 18 [-]

ASTM D395, 22 h

70.0 °C

26 [-]

Show Supplier Material materials with Compression set of 26 [-]

ASTM D395, 22 h

120.0 °C

43 [-]

Show Supplier Material materials with Compression set of 43 [-]

ASTM D395, 22 h

Elongation

23.0 °C

450 %

Show Supplier Material materials with Elongation of 450 %

ASTM D412

Hardness, Shore A

23.0 °C

65 - 69 [-]

Show Supplier Material materials with Hardness, Shore A of 65 - 69 [-]

ASTM 2240, for 5-15 seconds

Tear strength

23.0 °C

25 kN/m

Show Supplier Material materials with Tear strength of 25 kN/m

ASTM D624

Tensile strength

23.0 °C

6 MPa

Show Supplier Material materials with Tensile strength of 6 MPa

ASTM D412

Thermal

PropertyValueComment

Brittleness temperature

-60 °C

Show Supplier Material materials with Brittleness temperature of -60 °C

D746

Technological properties

Property
Processing methods

Extrusion: Hopper Temperature: 140-150°C, Middle Temperature: 150-170°C, Measurment Temperature: 170-190°C, Front Temperature: 180-200°C, Mold Temperature: 170-190°C, Melt Temperature: 160-180°C, Comp. Ratio:3:1, Screen: 20-60 Mesh - Injection: Rear Temperature: 150-170°C, Middle Temperature: 170-190°C, Front Temperature: 190-220°C, Nozzle Temperature: 190-210°C, Melt Temperature:180-200°C, Mold Temperature: 30-80°C, Speed: 100-200rpm, Back Pressure 0.07 - 0.7Mpa