ToughMet® 3AT Tube AT90 (C72900)

Alternative and trade names
ToughMet® 3AT Alloy
Want to keep this datasheet? Save it now in your required format

Description

ToughMet 3 AT alloy is a wrought, spinodally hardened copper alloy engineered for high strength and hardness. It resists mechanical wear, galling, stress relaxation, corrosion and erosion. ToughMet 3 alloy retains its strength at elevated temperature. It is non-magnetic and easy to machine into complex components.

Related Standards

This material data has been provided by Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

9 g/cm³

Show Supplier Material materials with Density of 9 g/cm³

Dimension

PropertyValue

Diameter

41 - 203 mm

Show Supplier Material materials with Diameter of 41 - 203 mm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

144 GPa

Show Supplier Material materials with Elastic modulus of 144 GPa

Elongation

23.0 °C

12 - 15 %

Show Supplier Material materials with Elongation of 12 - 15 %

Hardness, Rockwell C

23.0 °C

22 [-]

Show Supplier Material materials with Hardness, Rockwell C of 22 [-]

Poisson's ratio

23.0 °C

0.33 [-]

Show Supplier Material materials with Poisson's ratio of 0.33 [-]

Tensile strength

23.0 °C

760 MPa

Show Supplier Material materials with Tensile strength of 760 MPa

Yield strength Rp0.2

23.0 °C

620 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 620 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.64E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.64E-5 1/K

Thermal conductivity

23.0 °C

38 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 38 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical conductivity

23.0 °C

4.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m

max.

Specific Electrical conductivity

7 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS

max.

Magnetic

PropertyTemperatureValue

Relative magnetic permeability

23.0 °C

1 [-]

Show Supplier Material materials with Relative magnetic permeability of 1 [-]

Chemical properties

PropertyValue

Copper

Balance

Nickel

15 %

Show Supplier Material materials with Nickel of 15 %

Tin

8 %

Show Supplier Material materials with Tin of 8 %

Technological properties

Property
Application areas

ToughMet 3 AT alloy is used for bushings and bearings for commercial aircraft, high performance engines as well as mining, industrial and heavy equipment. It is also used to make oil and gas drilling hardware, including rotary steerable housings, kelly valve seats and pressure housings.

Surface Finish

Mill hardened finish