Módulo elástico: 13.36 GPa

Quick Comparison

Polyphenylene Sulfide (PPS)

Polyphenylene sulfide Reinforced with 40% Glass Fibre (PPS+GF40)

Suministrada por:

2 proveedores de Matmatch

Poliftalamida (PPA)

Polyphthalamide Reinforced with 33% Glass Fibre (PPA+GF33)

Suministrada por:

2 proveedores de Matmatch

Polyamide 66 (PA66)

Polyamide 66 Reinforced with 50% Glass Fibers (PA66+GF50)

Suministrada por:

4 proveedores de Matmatch

Polyamide 46 (PA46)

Polyamide 46 Reinforced with 50% Glass Fibers (PA46+GF50)

Suministrada por:

2 proveedores de Matmatch

Polímero

Liquid-crystalline polymer Reinforced with 30% Glass Fibers (LCP+GF30)

Suministrada por:

1 proveedor Matmatch

Polímero

Liquid-crystalline polymer (LCP)

Suministrada por:

1 proveedor Matmatch

Polímero

Liquid-crystalline polymer Reinforced with 40% Glass Fibers (LCP+GF40)

Suministrada por:

1 proveedor Matmatch

Polyamide 66 (PA66)

PA66 GF50 black HAKAmid

Suministrada por:

Aurora Kunststoffe GmbH

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RFB66 - Asia

Suministrada por:

Sabic