Description

It is is a 33% glass fiber reinforced Polyamide 46. It can be heat stabilized. It has a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.43 - 1.49 g/cm³

Show Material materials with Density of 1.43 - 1.49 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

11.5 - 14.0 GPa

Show Material materials with Elastic modulus of 11.5 - 14.0 GPa

Elongation

2.0 - 2.5 %

Show Material materials with Elongation of 2.0 - 2.5 %

Impact strength, Charpy notched

6.0 - 14.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6.0 - 14.0 kJ/m²

Impact strength, Charpy unnotched

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

50 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

Tensile strength

170.0 - 200.0 MPa

Show Material materials with Tensile strength of 170.0 - 200.0 MPa

at 2-2.5% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2.5e-05 - 7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5e-05 - 7e-05 1/K

Melting point

310.0 - 327.0 °C

Show Material materials with Melting point of 310.0 - 327.0 °C

Specific heat capacity

1200 J/(kg·K)

Show Material materials with Specific heat capacity of 1200 J/(kg·K)

Thermal conductivity

0.34 W/(m·K)

Show Material materials with Thermal conductivity of 0.34 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

3.4 [-]

Show Material materials with Dielectric constant of 3.4 [-]

4.7 [-]

Show Material materials with Dielectric constant of 4.7 [-]

Electrical resistivity

1000000000000.0 - 20000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000000.0 - 20000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

cell phones, connectors, housings, fuel lines

Fillers

33% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding