Polyamide 6T (PA6T)
Zytel® HTNFR52G45NHF BK337Polyphenylene Sulfide (PPS)
Polyphenylene sulfide Reinforced with 40% Glass Fibre (PPS+GF40)Suministrada por:
2 proveedores de Matmatch
Tereftalato de polibutileno (PBT)
Poly(butylene terephthalate) Reinforced with 50% Glass Fibers (PBT+GF50)Suministrada por:
4 proveedores de Matmatch
Polímero
Liquid-crystalline polymer Reinforced with 30% Glass Fibers (LCP+GF30)Suministrada por:
1 proveedor Matmatch
Polímero
Liquid-crystalline polymer Reinforced with 40% Glass Fibers (LCP+GF40)Suministrada por:
1 proveedor Matmatch
Tereftalato de polibutileno (PBT)
Crastin® SK609 BK851Madera
Moso Bamboo