Acero bajo en carbono
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Acero bajo en carbono
DIN 17155 Grade 17Mn4 normalized or normalized formed (+N)Chromium Molybdenum Steel
DIN 17175 Grade 14MoV6-3 quenched and tempered (+QT)Acero bajo en carbono
DIN 17115 Grade 15Mn3Al normalized or normalized formed (+N)Acero bajo en carbono
DIN 17115 Grade 21Mn4Al normalized or normalized formed (+N)Chromium Molybdenum Steel
DIN 17155 Grade 13CrMo4-4 quenched and tempered (+QT)Pure/Low Nickel Alloy
DIN 17740 Grade LC-Ni99 soft annealed (+A)Platino
PtW5 deformed conditionPure/Low Nickel Alloy
DIN 17740 Grade Ni99.2 soft annealed (+A)Aleación de níquel-hierro
DIN 17745 Grade NiFe48CrWrought Copper Nickel Grade
Niclal 43 (Strips, Rods, Wires) - CuMn12Ni4Suministrada por: