Acero bajo en carbono
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Unclassified Low Alloy Steel
EN 10025-6 Grade S690QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Acero bajo en carbono
EN 10216-2 Grade 19Mn5 normalized or normalized formed (+N)Acero bajo en carbono
EN 10250-2 Grade 20Mn5 quenched and tempered (+QT)Acero bajo en carbono
EN 10250-2 Grade 20Mn5 normalized and tempered (+NT)Acero bajo en carbono
EN 10250-2 Grade C25E normalized and tempered (+NT)Acero bajo en carbono
EN 10250-2 Grade C25E quenched and tempered (+QT)Acero inoxidable martensítico
DIN 17440 Grade X12Cr13 soft annealed (+A)Acero bajo en carbono
EN 10083-1 Grade C25E quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C25R quenched and tempered (+QT)Acero inoxidable martensítico
EN 10088-1 Grade X6Cr13 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X2CrTi17 soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X6Cr13 soft annealed (+A)Acero bajo en carbono
EN 10269 Grade 19MnB4 quenched and tempered (+QT)Acero bajo en carbono
EN 10269 Grade 20Mn5 normalized or normalized formed (+N)Acero inoxidable ferrítico
EN 10028-7 Grade X2CrNi12 soft annealed (+A)