Acero inoxidable ferrítico
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrTi17 soft annealed (+A)Acero inoxidable dúplex
EN 10088-1 Grade X2CrNiN23-4 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoCuN25-6-3 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiMoCuWN25-7-4 solution annealed (+AT)Acero inoxidable dúplex
EN 10028-7 Grade X2CrNiN23-4 solution annealed (+AT)Acero inoxidable ferrítico
EN 10028-7 Grade X3CrTi17 soft annealed (+A)Acero inoxidable dúplex
EN 10088-1 Grade X2CrNiMoCuN25-6-3 solution annealed (+AT)Acero inoxidable dúplex
EN 10088-1 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Acero inoxidable dúplex
DIN 5512-3 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Acero inoxidable ferrítico
EN 10028-7 Grade X6CrNiTi12 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X6CrNiTi12 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X2CrMoTi17-1 soft annealed (+A)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNbZr17 soft annealed (+A)Acero bajo en carbono
EN 10327 Grade DX55D hot dip aluminium-silicon coated (+AS)Acero bajo en carbono
EN 10327 Grade DX52D hot dip zinc, zinc-iron, zinc-aluminium, zinc-magnesium, aluminium-zinc or aluminium-silicon coated (+Z, +ZF, +ZA, +ZM, +AZ, +AS)