Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl® is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.

Datasheet URL:

Stanyl® HGR3-W (P1120D)

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

dry

ISO 1183

Moisture absorption

3.7 %

Show Supplier Material materials with Moisture absorption of 3.7 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

0.7 GPa

Show Supplier Material materials with Elastic modulus of 0.7 GPa

conditioned

ISO 527-1/-2

2.5 GPa

Show Supplier Material materials with Elastic modulus of 2.5 GPa

dry

ISO 527-1/-2

120 °C

0.56 GPa

Show Supplier Material materials with Elastic modulus of 0.56 GPa

dry

ISO 527-1/-2

Elongation

35 %

Show Supplier Material materials with Elongation of 35 %

dry

ISO 527-1/-2

120 °C

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

Elongation at yield

18 %

Show Supplier Material materials with Elongation at yield of 18 %

dry

ISO 527-1/-2

30 %

Show Supplier Material materials with Elongation at yield of 30 %

conditioned

ISO 527-1/-2

Flexural modulus

0.65 GPa

Show Supplier Material materials with Flexural modulus of 0.65 GPa

conditioned

ISO 178

2.4 GPa

Show Supplier Material materials with Flexural modulus of 2.4 GPa

dry

ISO 178

80 °C

0.8 GPa

Show Supplier Material materials with Flexural modulus of 0.8 GPa

dry

ISO 178

Flexural yield strength

19 MPa

Show Supplier Material materials with Flexural yield strength of 19 MPa

conditioned

ISO 178

93 MPa

Show Supplier Material materials with Flexural yield strength of 93 MPa

dry

ISO 178

80 °C

33 MPa

Show Supplier Material materials with Flexural yield strength of 33 MPa

dry

ISO 178

Impact strength, Charpy notched

-30 °C

14.0 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m²

dry

ISO 179/1eA

-30 °C

16 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m²

conditioned

ISO 179/1eA

23 °C

22 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 22 kJ/m²

dry

ISO 179/1eA

23 °C

130 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 130 kJ/m²

conditioned

ISO 179/1eA

Tensile strength

65 MPa

Show Supplier Material materials with Tensile strength of 65 MPa

dry

ISO 527-1/-2

120 °C

45 MPa

Show Supplier Material materials with Tensile strength of 45 MPa

dry

ISO 527-1/-2

Yield strength

40 MPa

Show Supplier Material materials with Yield strength of 40 MPa

conditioned

ISO 527-1/-2

75 MPa

Show Supplier Material materials with Yield strength of 75 MPa

dry

ISO 527-1/-2

120 °C

35 MPa

Show Supplier Material materials with Yield strength of 35 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Coefficient of thermal expansion

9e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K

dry

ISO 11359-1/-2

Parallel

1.1e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.1e-06 1/K

dry

ISO 11359-1/-2

Normal

Glass transition temperature

75 °C

Show Supplier Material materials with Glass transition temperature of 75 °C

dry

ISO 11357-1/-2

10°C/min

Melting point

295 °C

Show Supplier Material materials with Melting point of 295 °C

dry

ISO 11357-1/-3

10°C/min

Thermal diffusivity

9.82e-07 mm²/s

Show Supplier Material materials with Thermal diffusivity of 9.82e-07 mm²/s

dry

-

Rheological Properties

PropertyValueConditionTesting StandardComment

Density of melt

913 g/cm³

Show Supplier Material materials with Density of melt of 913 g/cm³

dry

-

Shrinkage

2 %

Show Supplier Material materials with Shrinkage of 2 %

dry

Sim. to ISO 294-4

Parallel

2 %

Show Supplier Material materials with Shrinkage of 2 %

dry

Sim. to ISO 294-4

Normal

Specific heat capacity melt

2550 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2550 J/(kg·K)

dry

-

Thermal conductivity of melt

0.24 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K)