Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch
Acero bajo en carbono
EN 10216-2 Grade 19Mn5 normalized or normalized formed (+N)Acero inoxidable austenítico
UGIMA® 4435 ICH Solution Annealed and Cold drawnSuministrada por:
UgitechAcero inoxidable austenítico
DIN 17445 Grade G-X5CrNiMoNb18-10 quenched (+Q)Chromium Molybdenum Steel
DIN 17175 Grade 14MoV6-3 quenched and tempered (+QT)Chromium Molybdenum Steel
DIN 17155 Grade 10CrMo9-10 quenched and tempered (+QT)Acero bajo en carbono
BS 970-1 Grade 070M20 NormalizedAcero bajo en carbono
EN 10277-2 Grade C10 as rolled and turned (+SH)Acero bajo en carbono
EN 10277-2 Grade C15 as rolled and turned (+SH)Acero bajo en carbono
EN 10277-4 Grade C15R as rolled and turned (+SH)Wrought Copper High Copper Alloy
EN 1652 Grade CuCo2Be THAcero bajo en carbono
DIN 1651 Grade 10S20 untreatedAcero bajo en carbono
ISO 683-4 Grade 10S20 untreatedAcero bajo en carbono
ISO 683-4 Grade 11SMn30 untreated