Dureza Brinell: 171 [-]

Quick Comparison

Acero inoxidable austenítico

UGI 4435 IRH Solution Annealed

Suministrada por:

Ugitech

Wrought Copper Bronze Silicon Bronze

COLSIBRO® Copper Alloy

Acero inoxidable austenítico

UGI 4404FGX3 Turned Bar

Suministrada por:

Ugitech

Acero inoxidable austenítico

UGI 4404FGX3 Drawn Bar

Suministrada por:

Ugitech

Acero inoxidable austenítico

UGIMA® 4435 ICH Solution Annealed and Cold drawn

Suministrada por:

Ugitech

Wrought Copper Nickel Silver Grade

ARCAP® AP4 H11 - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys

Wrought Copper Nickel Silver Grade

ARCAP® AP4 H12 - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys

Wrought Copper Bronze Aluminium Bronze

CA10 - CuAl7Si2 - C64200

Suministrada por:

Lebronze Alloys

Wrought Copper High Copper Alloy

EN 1652 Grade CuCo2Be TH

Acero bajo en carbono

DIN 1651 Grade 15S10 untreated
Página 1 de 19