Dureza Vickers: 223 [-]

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70260 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C52100 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51900 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Bronce fosforado

UNS C52400 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51100 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51000 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Bronce fosforado

UNS C51900 R640

Wrought Copper Bronze Aluminium Bronze

NC4 - CuAl10Ni5Fe4 - C63000 / C63200

Suministrada por:

Lebronze Alloys

Bronce fosforado

JIS C5240HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM00 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM02 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD01 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD02 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD04 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD04 Strip (C72700)

Suministrada por:

Materion Brush GmbH
Página 1 de 9