Heat deflection temperature, 1.80 MPa: 195 °C

Quick Comparison

Mezcla de polímeros

VALOX™ FR Resins 865

Polyamide 6 (PA6)

Akulon® K224-HG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HGR24

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G3

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 8018HS NC010

Polyamide 6 (PA6)

Akulon® Ultraflow K-FG5

Suministrada por:

DSM Engineering Materials

Tereftalato de polibutileno (PBT)

Arnite® TV4 230

Suministrada por:

DSM Engineering Materials

Tereftalato de polibutileno (PBT)

EPIMIX PBT GV0 15 NC Q1B5A901

Suministrada por:

EPSAN

Tereftalato de polibutileno (PBT)

EPIMIX PBT GV0 30 NC Q1D0B001

Suministrada por:

EPSAN

Polieterimida (PEI)

LNP™ THERMOCOMP™ Compound EC006PXQ

Suministrada por:

Sabic

Polieterimida (PEI)

LNP™ THERMOCOMP™ Compound EC006APQ

Suministrada por:

Sabic

Polyamide 6 (PA6)

Akulon® K224-G4

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

EPLAMID 6 CFR 30 BK Q1D001 (PA6)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFI 30 NC Q1D0A501 (PA6)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFI 30 NC Q1D0B001 (PA6)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFI 30 XCM NC Q1D0B801 (PA6)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFI 40 NC Q1E0A301 (PA6)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLON⁺ 6 GFR 30 BK Q2D004

Suministrada por:

EPSAN

Polyamide 6 (PA6)

LNP™ STAT-KON™ Compound PFD04S

Suministrada por:

Sabic

Polyamide 6 (PA6)

Akulon® K224-LG3

Suministrada por:

DSM Engineering Materials