General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.15 % Show Supplier Material materials with Moisture absorption of 2.15 % | dry | Sim. to ISO 62 |
Water absorption | 7.2 % Show Supplier Material materials with Water absorption of 7.2 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.3 GPa Show Supplier Material materials with Elastic modulus of 4.3 GPa | conditioned | ISO 527-1/-2 | |
7.3 GPa Show Supplier Material materials with Elastic modulus of 7.3 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
10 % Show Supplier Material materials with Elongation of 10 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 6.3 GPa Show Supplier Material materials with Flexural modulus of 6.3 GPa | dry | ISO 178 | |
Flexural yield strength | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 55.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 55.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 85 MPa Show Supplier Material materials with Tensile strength of 85 MPa | conditioned | ISO 527-1/-2 | |
145 MPa Show Supplier Material materials with Tensile strength of 145 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 195 °C Show Supplier Material materials with Heat deflection temperature of 195 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 9.83e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 9.83e-08 mm²/s | dry | - |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1090 g/cm³ Show Supplier Material materials with Density of melt of 1090 g/cm³ | dry | - | |
Shrinkage | 0.25 % Show Supplier Material materials with Shrinkage of 0.25 % | dry | ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Shrinkage of 1.1 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2340 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2340 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.25 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.25 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |