Temperatura de flexión bajo carga: 225 °C

Quick Comparison

Polyamide 6 (PA6)

LNP™ KONDUIT™ Compound PX11313

Suministrada por:

Sabic

Polyamide 66 (PA66)

Akulon® S223-E

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-EH

Suministrada por:

DSM Engineering Materials

Polietileno tereftalato (PET)

Arnite® AV2 370 XL

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF0029S

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ KONDUIT™ Compound OTF2B

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF002SXS

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF0039S

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF003ES

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006ESZ

Suministrada por:

Sabic

Polyamide 66 (PA66)

Akulon® SafeConnect SC21

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF005SXS

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

Arnite® TV4 261 KL

Suministrada por:

DSM Engineering Materials

Poliamida

EXTEM™ Resin XH1015 - Europe

Suministrada por:

Sabic

Poliamida

EXTEM™ Resin XH1015 - Asia

Suministrada por:

Sabic

Poliamida

EXTEM™ Resin XH1015 - Americas

Suministrada por:

Sabic

Mezcla de polímeros

Arnite® TV4 461 KL

Suministrada por:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

LNP™ STAT-KON™ Compound OEL13I

Suministrada por:

Sabic
Página 1 de 4