General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 8.6 GPa Show Supplier Material materials with Elastic modulus of 8.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 8.3 GPa Show Supplier Material materials with Flexural modulus of 8.3 GPa | ISO 178 |
Flexural strength | 23.0 °C | 205 MPa Show Supplier Material materials with Flexural strength of 205 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 33 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 485 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 485 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 6 J Show Supplier Material materials with Instrumented Impact, at Peak of 6 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 139 MPa Show Supplier Material materials with Tensile strength of 139 MPa | ISO 527 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 224 - 258 °C Show Supplier Material materials with Heat deflection temperature of 224 - 258 °C | ||
Heat deflection temperature, 0.45 MPa | 258 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 258 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 224 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 224 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101281586- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |