General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.53 g/cm³ Show Supplier Material materials with Density of 1.53 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 9.9 GPa Show Supplier Material materials with Elastic modulus of 9.9 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
225 °C Show Supplier Material materials with Heat deflection temperature of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 275 V Show Supplier Material materials with Comparative tracking index of 275 V | dry | IEC 60112 | |
Dielectric constant | 3.9 [-] Show Supplier Material materials with Dielectric constant of 3.9 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Dielectric constant of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dissipation factor | 15 [-] Show Supplier Material materials with Dissipation factor of 15 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Dissipation factor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Exterior Mirror Bases | |
Fillers | 30% Glass Fiber |