Policarbonato (PC)
LEXAN™ Healthcare Resin HP1Policarbonato (PC)
LEXAN™ Healthcare Resin HPS1RPolicarbonato (PC)
LEXAN™ Healthcare Resin HPS2Policarbonato (PC)
LEXAN™ Healthcare Resin HP1RAcrilonitrilo butadieno estireno (ABS)
CYCOLAC™ Resin MG94Acrilonitrilo butadieno estireno (ABS)
CYCOLAC™ Resin X11Mezcla de polímeros
XENOY™ Resin 1731Acrilonitrilo butadieno estireno (ABS)
CYCOLAC™ Resin MG94UPolicarbonato (PC)
LEXAN™ Resin EM3110