General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.17 - 0.28 [-] Show Supplier Material materials with Coefficient of friction of 0.17 - 0.28 [-] | ||
Coefficient of friction, kinetic | 0.28 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.28 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.17 [-] Show Supplier Material materials with Coefficient of friction, static of 0.17 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongation | 23.0 °C | 53 % Show Supplier Material materials with Elongation of 53 % | ASTM D 638 | break | ||
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ASTM D 790 | ||
Flexural strength | 23.0 °C | 81 MPa Show Supplier Material materials with Flexural strength of 81 MPa | ASTM D 790 | ||
Impact strength, Izod notched | 23.0 °C | 240 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 240 kJ/m² | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 240 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 240 J/m | ASTM D 256 | notched, 23°C | ||
Tensile strength | 23.0 °C | 53 MPa Show Supplier Material materials with Tensile strength of 53 MPa | ASTM D 638 | break | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 128 °C Show Supplier Material materials with Heat deflection temperature of 128 °C | ||
Heat deflection temperature, 1.80 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 128 °C | ASTM D 648 | 3.2mm, unannealed | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282870- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343861- - <br> UL Yellow Card Link 3: https://iq.ul.com/ul/cert.aspx?ULID=101344454- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Enclosure/Housing/Cover, Enclosures, Document Handling, Amusement Machine | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |