Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-20Suministrada por:
Arkema: High Performance PolymersPolyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-25Suministrada por:
Arkema: High Performance PolymersEtilvinilacetato
Ethylene Vinyl Acetate (EVAC) filled acoustical recyclateSuministrada por:
Heffco Elastomers Inc