Ethylene Vinyl Acetate (EVAC) filled acoustical recyclate

Want to keep this datasheet? Save it now in your required format

Description

Low fog filled thermoplastic ethylene polymer providing acoustical sound barrier performance in automotive, construction, and industrial applications.

This material data has been provided by Heffco Elastomers Inc..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting Standard

Density

1.9 g/cm³

Show Supplier Material materials with Density of 1.9 g/cm³

ASTM D792, ISO 1183

Mechanical

PropertyValueTesting Standard

Flexural modulus

0.110 GPa

Show Supplier Material materials with Flexural modulus of 0.110 GPa

ASTM D790

Hardness, Shore A

88 [-]

Show Supplier Material materials with Hardness, Shore A of 88 [-]

ASTM D2240, ISO 868

92 [-]

Show Supplier Material materials with Hardness, Shore A of 92 [-]

ASTM D2240, ISO 868

Tear strength

17.5 kN/m

Show Supplier Material materials with Tear strength of 17.5 kN/m

ASTM D624

Tensile strength

2.76 MPa

Show Supplier Material materials with Tensile strength of 2.76 MPa

ASTM D638, ISO 527-2

Rheological Properties

PropertyValueTesting StandardComment

Melt mass-flow rate

1.8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 1.8 g/10min

ASTM D1238, ISO 1183

190°C/2.16kg