Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedAcero inoxidable endurecido por precipitación
UNS S45500 AnnealedWrought Copper Pure / Low Alloyed Copper
CEN/TS 13388 Grade CW114C R250Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DLP O60Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuSP R250Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuSP R300Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuTeP R250Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuTeP R300Acero de alto carbono
EN 10132-4 Grade C75S Quenched and TemperedWrought Copper Pure / Low Alloyed Copper
CEN/TS 13388 Grade CW023A R200Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DLP R250Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DLP R300Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DLP R350Wrought Copper High Copper Alloy
EN 12164 Grade CuPb1P R250Wrought Copper High Copper Alloy
EN 12164 Grade CuPb1P R300Wrought Copper Pure / Low Alloyed Copper
EN 1652 Grade Cu-DLP R200Wrought Copper Pure / Low Alloyed Copper
EN 1652 Grade Cu-DLP R240Wrought Copper Pure / Low Alloyed Copper
EN 1652 Grade Cu-DLP R290Wrought Copper Pure / Low Alloyed Copper
EN 1653 Grade Cu-DLP R200Wrought Copper Pure / Low Alloyed Copper
EN 12164 Grade CuTeP R360