Wrought Copper Bronze Aluminium Bronze
AMPCO® 45 Extruded and drawn rodsSuministrada por:
AMPCO METALNickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Aleación alfa-beta
DIN 17851 Grade TiAl6V6Sn2 AnnealedNickel Chromium Iron Alloy
Alloy 718 Nickel AlloyNickel Chromium Alloy
DIN 17742 Grade NiCr20TiAl precipitation hardened (+P)Aleación alfa-beta
DIN 17851 Grade TiAl6V4 Artificially AgedSuministrada por:
5 proveedores de Matmatch
Acero inoxidable austenítico
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Aleación alfa-beta
DIN 17851 Grade TiAl6V6Sn2 Artificially AgedAcero bajo en carbono
ASTM A148 Grade 1450-1240 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedAcero bajo en carbono
ASTM A148 Grade 1450-1240L Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedAcero inoxidable martensítico
ASTM A705 Grade XM-12 Age-Hardening H900Acero bajo en carbono
JIS G3136 Grade SN490CAcero bajo en carbono
JIS G3136 Grade SN400C