Calor específico: 1380 J/(kg·K)

Quick Comparison

Polipropileno

Polypropylene Reinforced with 30% Glass Fibre (PP+GF30)

Suministrada por:

1 proveedor Matmatch

Polyphenylene Sulfide (PPS)

Polyphenylene sulfide Reinforced with 40% Glass Fibre (PPS+GF40)

Suministrada por:

2 proveedores de Matmatch

Polyamide 6 (PA6)

Polyamide 6 Reinforced with 50% Glass Fibers (PA6+GF50)

Suministrada por:

2 proveedores de Matmatch

Polyvinylidenefluoride (PVDF)

Polyvinylidene fluoride (PVDF)

Suministrada por:

2 proveedores de Matmatch

Copoliéster termoplástico

Copolyester thermoplastic elastomer (TPC)

Suministrada por:

1 proveedor Matmatch

Polipropileno

Polypropylene Reinforced with 30% Long Glass Fibers (PP+LGF30)

Suministrada por:

1 proveedor Matmatch

Caucho de fluorosilicona (FVMQ)

Fluorine silicone rubber (FVMQ)