General
Property | Value |
---|---|
Density | 1.19 - 1.21 g/cm³ Show Material materials with Density of 1.19 - 1.21 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 2.1 - 2.4 GPa Show Material materials with Elastic modulus of 2.1 - 2.4 GPa | ||
Elongation | 35.0 - 50.0 % Show Material materials with Elongation of 35.0 - 50.0 % | ||
Impact strength, Charpy notched | 6.0 - 20.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 6.0 - 20.0 kJ/m² | ||
Tensile strength | 20.0 - 40.0 MPa Show Material materials with Tensile strength of 20.0 - 40.0 MPa | at 3.5-4.5% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00011 - 0.00015 1/K Show Material materials with Coefficient of thermal expansion of 0.00011 - 0.00015 1/K |
Specific heat capacity | 1200.0 - 1900.0 J/(kg·K) Show Material materials with Specific heat capacity of 1200.0 - 1900.0 J/(kg·K) |
Thermal conductivity | 0.21 W/(m·K) Show Material materials with Thermal conductivity of 0.21 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 3.55 [-] Show Material materials with Dielectric constant of 3.55 [-] |
4.2 [-] Show Material materials with Dielectric constant of 4.2 [-] | |
Electrical resistivity | 10000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 10000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Model railway components, eye glasses, stencils, toothbrushes | |
Processing methods | Injection molding, extrusion, rotational molding |