Polyamide 6 Reinforced with 50% Glass Fibers (PA6+GF50)

Alternative and trade names
Zytel®, Ultramid®, Durethan®, Radilon®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced Polyamide 6 with 50% glass fiber. Different grades availbale heat-aging stabilized,improved surface finish, weather stabilized.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.54 - 1.58 g/cm³

Show Material materials with Density of 1.54 - 1.58 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

9.5 - 12.5 GPa

Show Material materials with Elastic modulus of 9.5 - 12.5 GPa

Elongation

3.0 - 6.0 %

Show Material materials with Elongation of 3.0 - 6.0 %

Impact strength, Charpy notched

20.0 - 40.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 20.0 - 40.0 kJ/m²

Impact strength, Charpy unnotched

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

110 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 110 kJ/m²

Tensile strength

130.0 - 180.0 MPa

Show Material materials with Tensile strength of 130.0 - 180.0 MPa

at 3-6% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1e-05 - 0.0001 1/K

Show Material materials with Coefficient of thermal expansion of 1e-05 - 0.0001 1/K

Melting point

220.0 - 223.0 °C

Show Material materials with Melting point of 220.0 - 223.0 °C

Specific heat capacity

1300.0 - 1950.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1300.0 - 1950.0 J/(kg·K)

Thermal conductivity

0.28 W/(m·K)

Show Material materials with Thermal conductivity of 0.28 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

5 [-]

Show Material materials with Dielectric constant of 5 [-]

14 [-]

Show Material materials with Dielectric constant of 14 [-]

Electrical resistivity

1000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Power tool housings, cattle ear taggers, luggage frames, fans, pressure regulator housings

Fillers

50% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, extrusion