Poly Acrylonitrile Copolymer Powder N-PAN (AN316010)

Alternative and trade names
Poly Acrylonitrile Copolymer Powder N-PAN (AN316010)
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

0.34 - 0.39 g/cm³

Show Material materials with Bulk density of 0.34 - 0.39 g/cm³

DIN ISO 697

Density

1.18 g/cm³

Show Material materials with Density of 1.18 g/cm³

Diffusion coefficient

4e-16 cm²/s

Show Material materials with Diffusion coefficient of 4e-16 cm²/s

Exterior surface area

0.14800000000000002 m²/g

Show Material materials with Exterior surface area of 0.14800000000000002 m²/g

globular particles assumed

Fikentscher K value

83.5 [-]

Show Material materials with Fikentscher K value of 83.5 [-]

Free acid groups

0.5 N/kg

Show Material materials with Free acid groups of 0.5 N/kg

N = milliequivalents

1 N/kg

Show Material materials with Free acid groups of 1 N/kg

N = milliequivalents

Molar mass

85000.0 g/mol

Show Material materials with Molar mass of 85000.0 g/mol

Particle size D50

46.1 μm

Show Material materials with Particle size D50 of 46.1 μm

mesh 120

Residual monomer

150 mg/kg

Show Material materials with Residual monomer of 150 mg/kg

300 mg/kg

Show Material materials with Residual monomer of 300 mg/kg

Total acid groups

55 N/kg

Show Material materials with Total acid groups of 55 N/kg

N = milliequivalents

59 N/kg

Show Material materials with Total acid groups of 59 N/kg

N = milliequivalents

Water absorption

22 °C

2.5 %

Show Material materials with Water absorption of 2.5 %

95 % rel. humidity

Water retention

84.0 %

Show Material materials with Water retention of 84.0 %

DIN 53814

pH Value

6.7 - 7.3 [-]

Show Material materials with pH Value of 6.7 - 7.3 [-]

of a 25 vol. % aqueous slurry

Thermal

PropertyValueComment

Combustion heat

-30.7 kJ/g

Show Material materials with Combustion heat of -30.7 kJ/g

Decomposition heat

-640.0 J/g

Show Material materials with Decomposition heat of -640.0 J/g

at 3K/min

Specific heat capacity

1200.0 - 1500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1200.0 - 1500.0 J/(kg·K)

Thermal conductivity

0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.2 W/(m·K)

Vicat softening temperature

180.0 °C

Show Material materials with Vicat softening temperature of 180.0 °C

Electrical

PropertyTemperatureValueComment

Dielectric constant

6.5 [-]

Show Material materials with Dielectric constant of 6.5 [-]

at 60Hz

Electrical conductivity

0.0045000000000000005 S/m

Show Material materials with Electrical conductivity of 0.0045000000000000005 S/m

of a 25 vol. % aqueous slurry

Electrical resistivity

20 °C

5000000 Ω·m

Show Material materials with Electrical resistivity of 5000000 Ω·m

at 65% relative humidity

Rheological Properties

PropertyValueComment

Specific Viscosity

920 [-]

Show Material materials with Specific Viscosity of 920 [-]

0.5% in DMF

960 [-]

Show Material materials with Specific Viscosity of 960 [-]

0.5% in DMF

Chemical properties

PropertyValueComment

Chlorine

0.001 %

Show Material materials with Chlorine of 0.001 %

Iron

0.0002 - 0.0004 %

Show Material materials with Iron of 0.0002 - 0.0004 %

Potassium

0.04 - 0.055 %

Show Material materials with Potassium of 0.04 - 0.055 %

Sodium

0.1 - 0.12 %

Show Material materials with Sodium of 0.1 - 0.12 %

Sulfur

0.2 - 0.22 %

Show Material materials with Sulfur of 0.2 - 0.22 %

according to Schöninger

Technological properties

Property
Color

Loose light white powder

Other

Co-monomer: 5.8% methyl acrylate, 0.3% methyl sulfonate; Networking not detectable