Resistencia a la tracción: 815 MPa

Quick Comparison

Acero bajo en carbono

EN 10025-2 Grade E360 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Acero bajo en carbono

ASTM A517 Grade F Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QL2 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Página 1 de 56