Polypropylene Reinforced with 40% Mineral (PP+M40)

Alternative and trade names
Polyfort™, Hostacom®, TECACOMP®, ALFAFIL®
Want to keep this datasheet? Save it now in your required format

Description

It is a 40% mineral filled PP homopolymer with high or low flow, high stiffness and low warpage. It is not intended for medical, pharmaceutical, food and drinking water applications.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.2 - 1.25 g/cm³

Show Material materials with Density of 1.2 - 1.25 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

2.5 - 4.3 GPa

Show Material materials with Elastic modulus of 2.5 - 4.3 GPa

Elongation

3.0 - 30.0 %

Show Material materials with Elongation of 3.0 - 30.0 %

Impact strength, Charpy notched

2.0 - 8.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 2.0 - 8.0 kJ/m²

Impact strength, Charpy unnotched

20 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

50 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

Tensile strength

22.0 - 40.0 MPa

Show Material materials with Tensile strength of 22.0 - 40.0 MPa

at 3-7% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.00008 1/K

Show Material materials with Coefficient of thermal expansion of 0.00008 1/K

Melting point

160.0 - 168.0 °C

Show Material materials with Melting point of 160.0 - 168.0 °C

Specific heat capacity

1390 J/(kg·K)

Show Material materials with Specific heat capacity of 1390 J/(kg·K)

Thermal conductivity

0.56 W/(m·K)

Show Material materials with Thermal conductivity of 0.56 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

2.8 [-]

Show Material materials with Dielectric constant of 2.8 [-]

3 [-]

Show Material materials with Dielectric constant of 3 [-]

Electrical resistivity

10000000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 10000000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Under the bonnet components, air conditioning parts, heater housings

Fillers

40% Mineral Powder

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, extrusion