Difusividad térmica: 6 mm²/s

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Suministrada por:

1 proveedor Matmatch

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Steel

ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Acero inoxidable austenítico

DIN 17440 Grade X2CrNiN18-10 quenched (+Q)

Acero inoxidable austenítico

DIN 17440 Grade X6CrNiTi18-10 quenched (+Q)

Acero inoxidable austenítico

DIN 17440 Grade X6CrNiNb18-10 quenched (+Q)

Acero inoxidable austenítico

EN 10272 Grade X6CrNiTi18-10 solution annealed (+AT)

Suministrada por:

5 proveedores de Matmatch

Página 1 de 15