EN 10272 Grade X6CrNiTi18-10 solution annealed (+AT)

Want to keep this datasheet? Save it now in your required format

Description

Steel grade X6CrNiTi18-10 acc. to DIN EN 10272 : 2001-01is used for hot and cold formed rods for pressure vessels. the material is the stabilized by Ti option of 1.4301 (X5CrNi18-10). The steel is therefore resistant to intercrystalline corrosion also on sensitized condition. The steel is unsuitable for mirror finishing due to Ti-addition.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20.0 °C

7.93 g/cm³

Show Material materials with Density of 7.93 g/cm³

solution annealed (+AT)

EN 10272

Bar

20.0 °C

7.9 g/cm³

Show Material materials with Density of 7.9 g/cm³

solution annealed (+AT)

EN 10272

Bar

20.0 °C

7.9 - 7.93 g/cm³

Show Material materials with Density of 7.9 - 7.93 g/cm³

solution annealed (+AT)

EN 10272

Bar

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

20.0 °C

200.0 GPa

Show Material materials with Elastic modulus of 200.0 GPa

solution annealed (+AT)

EN 10272

Bar

20.0 °C

196.0 - 200.0 GPa

Show Material materials with Elastic modulus of 196.0 - 200.0 GPa

solution annealed (+AT)

EN 10272

Bar

20.0 °C

199.26 - 200.0 GPa

Show Material materials with Elastic modulus of 199.26 - 200.0 GPa

solution annealed (+AT)

EN 10272

Bar

20.0 °C

196.0 GPa

Show Material materials with Elastic modulus of 196.0 GPa

solution annealed (+AT)

EN 10272

Bar

20.0 °C

196.0 - 199.26 GPa

Show Material materials with Elastic modulus of 196.0 - 199.26 GPa

solution annealed (+AT)

EN 10272

Bar

20.0 °C

199.26 GPa

Show Material materials with Elastic modulus of 199.26 GPa

solution annealed (+AT)

EN 10272

Bar

100.0 °C

194.0 GPa

Show Material materials with Elastic modulus of 194.0 GPa

solution annealed (+AT)

EN 10272

Bar

100.0 °C

190.0 - 194.0 GPa

Show Material materials with Elastic modulus of 190.0 - 194.0 GPa

solution annealed (+AT)

EN 10272

Bar

100.0 °C

190.0 GPa

Show Material materials with Elastic modulus of 190.0 GPa

solution annealed (+AT)

EN 10272

Bar

200.0 °C

186.0 GPa

Show Material materials with Elastic modulus of 186.0 GPa

solution annealed (+AT)

EN 10272

Bar

200.0 °C

182.0 - 186.0 GPa

Show Material materials with Elastic modulus of 182.0 - 186.0 GPa

solution annealed (+AT)

EN 10272

Bar

200.0 °C

182.0 GPa

Show Material materials with Elastic modulus of 182.0 GPa

solution annealed (+AT)

EN 10272

Bar

300.0 °C

179.0 GPa

Show Material materials with Elastic modulus of 179.0 GPa

solution annealed (+AT)

EN 10272

Bar

300.0 °C

174.0 - 179.0 GPa

Show Material materials with Elastic modulus of 174.0 - 179.0 GPa

solution annealed (+AT)

EN 10272

Bar

300.0 °C

174.0 GPa

Show Material materials with Elastic modulus of 174.0 GPa

solution annealed (+AT)

EN 10272

Bar

400.0 °C

172.0 GPa

Show Material materials with Elastic modulus of 172.0 GPa

solution annealed (+AT)

EN 10272

Bar

400.0 °C

166.0 - 172.0 GPa

Show Material materials with Elastic modulus of 166.0 - 172.0 GPa

solution annealed (+AT)

EN 10272

Bar

400.0 °C

166.0 GPa

Show Material materials with Elastic modulus of 166.0 GPa

solution annealed (+AT)

EN 10272

Bar

500.0 °C

165.0 GPa

Show Material materials with Elastic modulus of 165.0 GPa

solution annealed (+AT)

EN 10272

Bar

500.0 °C

158.0 - 165.0 GPa

Show Material materials with Elastic modulus of 158.0 - 165.0 GPa

solution annealed (+AT)

EN 10272

Bar

500.0 °C

158.0 GPa

Show Material materials with Elastic modulus of 158.0 GPa

solution annealed (+AT)

EN 10272

Bar

-100.0 °C

206.0 GPa

Show Material materials with Elastic modulus of 206.0 GPa

solution annealed (+AT)

EN 10272

Bar

600.0 °C

150.0 GPa

Show Material materials with Elastic modulus of 150.0 GPa

solution annealed (+AT)

EN 10272

Bar

700.0 °C

142.0 GPa

Show Material materials with Elastic modulus of 142.0 GPa

solution annealed (+AT)

EN 10272

Bar

800.0 °C

134.0 GPa

Show Material materials with Elastic modulus of 134.0 GPa

solution annealed (+AT)

EN 10272

Bar

900.0 °C

127.0 GPa

Show Material materials with Elastic modulus of 127.0 GPa

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

120.0 GPa

Show Material materials with Elastic modulus of 120.0 GPa

solution annealed (+AT)

EN 10272

Bar

95.0 °C

193.05 GPa

Show Material materials with Elastic modulus of 193.05 GPa

solution annealed (+AT)

EN 10272

Bar

150.0 °C

188.23 GPa

Show Material materials with Elastic modulus of 188.23 GPa

solution annealed (+AT)

EN 10272

Bar

205.0 °C

182.71 GPa

Show Material materials with Elastic modulus of 182.71 GPa

solution annealed (+AT)

EN 10272

Bar

260.0 °C

177.88 GPa

Show Material materials with Elastic modulus of 177.88 GPa

solution annealed (+AT)

EN 10272

Bar

315.0 °C

174.44 GPa

Show Material materials with Elastic modulus of 174.44 GPa

solution annealed (+AT)

EN 10272

Bar

370.0 °C

168.92 GPa

Show Material materials with Elastic modulus of 168.92 GPa

solution annealed (+AT)

EN 10272

Bar

425.0 °C

164.1 GPa

Show Material materials with Elastic modulus of 164.1 GPa

solution annealed (+AT)

EN 10272

Bar

485.0 °C

159.96 GPa

Show Material materials with Elastic modulus of 159.96 GPa

solution annealed (+AT)

EN 10272

Bar

540.0 °C

155.13 GPa

Show Material materials with Elastic modulus of 155.13 GPa

solution annealed (+AT)

EN 10272

Bar

595.0 °C

151.0 GPa

Show Material materials with Elastic modulus of 151.0 GPa

solution annealed (+AT)

EN 10272

Bar

650.0 °C

146.17 GPa

Show Material materials with Elastic modulus of 146.17 GPa

solution annealed (+AT)

EN 10272

Bar

705.0 °C

140.65 GPa

Show Material materials with Elastic modulus of 140.65 GPa

solution annealed (+AT)

EN 10272

Bar

760.0 °C

135.83 GPa

Show Material materials with Elastic modulus of 135.83 GPa

solution annealed (+AT)

EN 10272

Bar

815.0 °C

131.69 GPa

Show Material materials with Elastic modulus of 131.69 GPa

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Elongation

20.0 °C

30.0 %

Show Material materials with Elongation of 30.0 %

solution annealed (+AT)

EN 10272

Bar

Transverse

20.0 °C

40.0 %

Show Material materials with Elongation of 40.0 %

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Hardness, Brinell

20.0 °C

215.0

Show Material materials with Hardness, Brinell of 215.0

solution annealed (+AT)

EN 10272

Bar

Transverse

20.0 °C

215.0

Show Material materials with Hardness, Brinell of 215.0

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

solution annealed (+AT)

EN 10272

Bar

95.0 °C

0.296 [-]

Show Material materials with Poisson's ratio of 0.296 [-]

solution annealed (+AT)

EN 10272

Bar

150.0 °C

0.288 [-]

Show Material materials with Poisson's ratio of 0.288 [-]

solution annealed (+AT)

EN 10272

Bar

205.0 °C

0.286 [-]

Show Material materials with Poisson's ratio of 0.286 [-]

solution annealed (+AT)

EN 10272

Bar

260.0 °C, 370.0 °C

0.303 [-]

Show Material materials with Poisson's ratio of 0.303 [-]

solution annealed (+AT)

EN 10272

Bar

315.0 °C

0.304 [-]

Show Material materials with Poisson's ratio of 0.304 [-]

solution annealed (+AT)

EN 10272

Bar

425.0 °C

0.308 [-]

Show Material materials with Poisson's ratio of 0.308 [-]

solution annealed (+AT)

EN 10272

Bar

485.0 °C

0.318 [-]

Show Material materials with Poisson's ratio of 0.318 [-]

solution annealed (+AT)

EN 10272

Bar

540.0 °C

0.323 [-]

Show Material materials with Poisson's ratio of 0.323 [-]

solution annealed (+AT)

EN 10272

Bar

595.0 °C

0.335 [-]

Show Material materials with Poisson's ratio of 0.335 [-]

solution annealed (+AT)

EN 10272

Bar

650.0 °C

0.342 [-]

Show Material materials with Poisson's ratio of 0.342 [-]

solution annealed (+AT)

EN 10272

Bar

705.0 °C

0.325 [-]

Show Material materials with Poisson's ratio of 0.325 [-]

solution annealed (+AT)

EN 10272

Bar

760.0 °C

0.331 [-]

Show Material materials with Poisson's ratio of 0.331 [-]

solution annealed (+AT)

EN 10272

Bar

815.0 °C

0.345 [-]

Show Material materials with Poisson's ratio of 0.345 [-]

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Shear modulus

20.0 °C

77.22 GPa

Show Material materials with Shear modulus of 77.22 GPa

solution annealed (+AT)

EN 10272

Bar

95.0 °C

74.46 GPa

Show Material materials with Shear modulus of 74.46 GPa

solution annealed (+AT)

EN 10272

Bar

150.0 °C

73.08 GPa

Show Material materials with Shear modulus of 73.08 GPa

solution annealed (+AT)

EN 10272

Bar

205.0 °C

71.02 GPa

Show Material materials with Shear modulus of 71.02 GPa

solution annealed (+AT)

EN 10272

Bar

260.0 °C

68.26 GPa

Show Material materials with Shear modulus of 68.26 GPa

solution annealed (+AT)

EN 10272

Bar

315.0 °C

66.88 GPa

Show Material materials with Shear modulus of 66.88 GPa

solution annealed (+AT)

EN 10272

Bar

370.0 °C

64.81 GPa

Show Material materials with Shear modulus of 64.81 GPa

solution annealed (+AT)

EN 10272

Bar

425.0 °C

62.74 GPa

Show Material materials with Shear modulus of 62.74 GPa

solution annealed (+AT)

EN 10272

Bar

485.0 °C

60.67 GPa

Show Material materials with Shear modulus of 60.67 GPa

solution annealed (+AT)

EN 10272

Bar

540.0 °C

58.61 GPa

Show Material materials with Shear modulus of 58.61 GPa

solution annealed (+AT)

EN 10272

Bar

595.0 °C

56.54 GPa

Show Material materials with Shear modulus of 56.54 GPa

solution annealed (+AT)

EN 10272

Bar

650.0 °C

54.47 GPa

Show Material materials with Shear modulus of 54.47 GPa

solution annealed (+AT)

EN 10272

Bar

705.0 °C

53.09 GPa

Show Material materials with Shear modulus of 53.09 GPa

solution annealed (+AT)

EN 10272

Bar

760.0 °C

51.02 GPa

Show Material materials with Shear modulus of 51.02 GPa

solution annealed (+AT)

EN 10272

Bar

815.0 °C

48.95 GPa

Show Material materials with Shear modulus of 48.95 GPa

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Tensile strength

20.0 °C

500.0 - 700.0 MPa

Show Material materials with Tensile strength of 500.0 - 700.0 MPa

solution annealed (+AT)

EN 10272

Bar

Transverse

20.0 °C

500.0 - 700.0 MPa

Show Material materials with Tensile strength of 500.0 - 700.0 MPa

solution annealed (+AT)

EN 10272

Bar

100.0 °C

440.0 MPa

Show Material materials with Tensile strength of 440.0 MPa

solution annealed (+AT)

EN 10272

Bar

150.0 °C

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

solution annealed (+AT)

EN 10272

Bar

200.0 °C

390.0 MPa

Show Material materials with Tensile strength of 390.0 MPa

solution annealed (+AT)

EN 10272

Bar

250.0 °C

385.0 MPa

Show Material materials with Tensile strength of 385.0 MPa

solution annealed (+AT)

EN 10272

Bar

300.0 °C, 350.0 °C, 400.0 °C

375.0 MPa

Show Material materials with Tensile strength of 375.0 MPa

solution annealed (+AT)

EN 10272

Bar

450.0 °C

370.0 MPa

Show Material materials with Tensile strength of 370.0 MPa

solution annealed (+AT)

EN 10272

Bar

500.0 °C

360.0 MPa

Show Material materials with Tensile strength of 360.0 MPa

solution annealed (+AT)

EN 10272

Bar

550.0 °C

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100.0 °C

1.6e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 1/K

solution annealed (+AT)

EN 10272

Bar

100.0 °C

1.6e-05 - 1.67e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.67e-05 1/K

solution annealed (+AT)

EN 10272

Bar

100.0 °C

1.67e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.67e-05 1/K

solution annealed (+AT)

EN 10272

Bar

200.0 °C

1.65e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.65e-05 1/K

solution annealed (+AT)

EN 10272

Bar

200.0 °C

1.65e-05 - 1.72e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.65e-05 - 1.72e-05 1/K

solution annealed (+AT)

EN 10272

Bar

200.0 °C

1.72e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.72e-05 1/K

solution annealed (+AT)

EN 10272

Bar

300.0 °C

1.7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.7e-05 1/K

solution annealed (+AT)

EN 10272

Bar

300.0 °C

1.7e-05 - 1.77e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.7e-05 - 1.77e-05 1/K

solution annealed (+AT)

EN 10272

Bar

300.0 °C

1.77e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.77e-05 1/K

solution annealed (+AT)

EN 10272

Bar

400.0 °C

1.75e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.75e-05 1/K

solution annealed (+AT)

EN 10272

Bar

400.0 °C

1.75e-05 - 1.81e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.75e-05 - 1.81e-05 1/K

solution annealed (+AT)

EN 10272

Bar

400.0 °C

1.81e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.81e-05 1/K

solution annealed (+AT)

EN 10272

Bar

500.0 °C

1.8e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.8e-05 1/K

solution annealed (+AT)

EN 10272

Bar

500.0 °C

1.8e-05 - 1.84e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.8e-05 - 1.84e-05 1/K

solution annealed (+AT)

EN 10272

Bar

500.0 °C

1.84e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.84e-05 1/K

solution annealed (+AT)

EN 10272

Bar

-100.0 °C

1.49e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.49e-05 1/K

solution annealed (+AT)

EN 10272

Bar

20.0 °C

1.61e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.61e-05 1/K

solution annealed (+AT)

EN 10272

Bar

600.0 °C

1.88e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.88e-05 1/K

solution annealed (+AT)

EN 10272

Bar

700.0 °C

1.91e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.91e-05 1/K

solution annealed (+AT)

EN 10272

Bar

800.0 °C

1.94e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.94e-05 1/K

solution annealed (+AT)

EN 10272

Bar

900.0 °C

1.97e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.97e-05 1/K

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 1/K

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Melting point

1230.0 - 1480.0 °C

Show Material materials with Melting point of 1230.0 - 1480.0 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

20.0 °C

500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 500.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

20.0 °C

472.0 - 500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 472.0 - 500.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

20.0 °C

472.0 J/(kg·K)

Show Material materials with Specific heat capacity of 472.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

-100.0 °C

440.0 J/(kg·K)

Show Material materials with Specific heat capacity of 440.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

100.0 °C

487.0 J/(kg·K)

Show Material materials with Specific heat capacity of 487.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

200.0 °C

503.0 J/(kg·K)

Show Material materials with Specific heat capacity of 503.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

300.0 °C

512.0 J/(kg·K)

Show Material materials with Specific heat capacity of 512.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

400.0 °C

520.0 J/(kg·K)

Show Material materials with Specific heat capacity of 520.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

500.0 °C

530.0 J/(kg·K)

Show Material materials with Specific heat capacity of 530.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

600.0 °C

541.0 J/(kg·K)

Show Material materials with Specific heat capacity of 541.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

700.0 °C

551.0 J/(kg·K)

Show Material materials with Specific heat capacity of 551.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

800.0 °C

559.0 J/(kg·K)

Show Material materials with Specific heat capacity of 559.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

900.0 °C

565.0 J/(kg·K)

Show Material materials with Specific heat capacity of 565.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

571.0 J/(kg·K)

Show Material materials with Specific heat capacity of 571.0 J/(kg·K)

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Thermal conductivity

20.0 °C

15.0 W/(m·K)

Show Material materials with Thermal conductivity of 15.0 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

20.0 °C

14.3 - 15.0 W/(m·K)

Show Material materials with Thermal conductivity of 14.3 - 15.0 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

20.0 °C

14.3 W/(m·K)

Show Material materials with Thermal conductivity of 14.3 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

100.0 °C

15.8 W/(m·K)

Show Material materials with Thermal conductivity of 15.8 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

200.0 °C

17.5 W/(m·K)

Show Material materials with Thermal conductivity of 17.5 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

300.0 °C

19.0 W/(m·K)

Show Material materials with Thermal conductivity of 19.0 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

400.0 °C

20.5 W/(m·K)

Show Material materials with Thermal conductivity of 20.5 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

500.0 °C

21.9 W/(m·K)

Show Material materials with Thermal conductivity of 21.9 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

600.0 °C

23.3 W/(m·K)

Show Material materials with Thermal conductivity of 23.3 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

700.0 °C

24.6 W/(m·K)

Show Material materials with Thermal conductivity of 24.6 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

800.0 °C

26.0 W/(m·K)

Show Material materials with Thermal conductivity of 26.0 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

900.0 °C

27.4 W/(m·K)

Show Material materials with Thermal conductivity of 27.4 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

28.8 W/(m·K)

Show Material materials with Thermal conductivity of 28.8 W/(m·K)

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Thermal diffusivity

20.0 °C

3.8 mm²/s

Show Material materials with Thermal diffusivity of 3.8 mm²/s

solution annealed (+AT)

EN 10272

Bar

100.0 °C

4.0 mm²/s

Show Material materials with Thermal diffusivity of 4.0 mm²/s

solution annealed (+AT)

EN 10272

Bar

200.0 °C

4.2 mm²/s

Show Material materials with Thermal diffusivity of 4.2 mm²/s

solution annealed (+AT)

EN 10272

Bar

300.0 °C

4.6 mm²/s

Show Material materials with Thermal diffusivity of 4.6 mm²/s

solution annealed (+AT)

EN 10272

Bar

400.0 °C

4.8 mm²/s

Show Material materials with Thermal diffusivity of 4.8 mm²/s

solution annealed (+AT)

EN 10272

Bar

500.0 °C

4.9 mm²/s

Show Material materials with Thermal diffusivity of 4.9 mm²/s

solution annealed (+AT)

EN 10272

Bar

600.0 °C

5.0 mm²/s

Show Material materials with Thermal diffusivity of 5.0 mm²/s

solution annealed (+AT)

EN 10272

Bar

700.0 °C

5.3 mm²/s

Show Material materials with Thermal diffusivity of 5.3 mm²/s

solution annealed (+AT)

EN 10272

Bar

800.0 °C

5.6 mm²/s

Show Material materials with Thermal diffusivity of 5.6 mm²/s

solution annealed (+AT)

EN 10272

Bar

900.0 °C

5.9 mm²/s

Show Material materials with Thermal diffusivity of 5.9 mm²/s

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

6.0 mm²/s

Show Material materials with Thermal diffusivity of 6.0 mm²/s

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical resistivity

20.0 °C

7.3e-07 Ω·m

Show Material materials with Electrical resistivity of 7.3e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

20.0 °C

7.1e-07 - 7.3e-07 Ω·m

Show Material materials with Electrical resistivity of 7.1e-07 - 7.3e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

20.0 °C

7.1e-07 Ω·m

Show Material materials with Electrical resistivity of 7.1e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

100.0 °C

7.76e-07 Ω·m

Show Material materials with Electrical resistivity of 7.76e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

200.0 °C

8.49e-07 Ω·m

Show Material materials with Electrical resistivity of 8.49e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

300.0 °C

9.14e-07 Ω·m

Show Material materials with Electrical resistivity of 9.14e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

400.0 °C

9.71e-07 Ω·m

Show Material materials with Electrical resistivity of 9.71e-07 Ω·m

solution annealed (+AT)

EN 10272

Bar

500.0 °C

1.022e-06 Ω·m

Show Material materials with Electrical resistivity of 1.022e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

600.0 °C

1.066e-06 Ω·m

Show Material materials with Electrical resistivity of 1.066e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

700.0 °C

1.104e-06 Ω·m

Show Material materials with Electrical resistivity of 1.104e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

800.0 °C

1.137e-06 Ω·m

Show Material materials with Electrical resistivity of 1.137e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

900.0 °C

1.166e-06 Ω·m

Show Material materials with Electrical resistivity of 1.166e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

1000.0 °C

1.191e-06 Ω·m

Show Material materials with Electrical resistivity of 1.191e-06 Ω·m

solution annealed (+AT)

EN 10272

Bar

Unlock all property charts

Chemical properties

PropertyValueConditionRelated StandardsShape

Carbon

0.08

Show Material materials with Carbon of 0.08

solution annealed (+AT)

EN 10272

Bar

Chromium

17.0 - 19.0 %

Show Material materials with Chromium of 17.0 - 19.0 %

solution annealed (+AT)

EN 10272

Bar

Manganese

2.0

Show Material materials with Manganese of 2.0

solution annealed (+AT)

EN 10272

Bar

Nickel

9.0 - 12.0 %

Show Material materials with Nickel of 9.0 - 12.0 %

solution annealed (+AT)

EN 10272

Bar

Phosphorus

0.045

Show Material materials with Phosphorus of 0.045

solution annealed (+AT)

EN 10272

Bar

Silicon

1.0

Show Material materials with Silicon of 1.0

solution annealed (+AT)

EN 10272

Bar

Sulfur

0.03

Show Material materials with Sulfur of 0.03

solution annealed (+AT)

EN 10272

Bar

0.015

Show Material materials with Sulfur of 0.015

solution annealed (+AT)

EN 10272

Bar

Titanium

0.7

Show Material materials with Titanium of 0.7

solution annealed (+AT)

EN 10272

Bar