Límite elástico Rp 0,2: 429 MPa

Quick Comparison

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NH normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10028-6 Grade P460QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P500QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Suministrada por:

3 proveedores de Matmatch

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

7000 Serie

AA Standards Grade 7075 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T651

Suministrada por:

3 proveedores de Matmatch

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

2000 Serie

AA Standards Grade 2024 T861

Suministrada por:

1 proveedor Matmatch

7000 Serie

AA Standards Grade 7075 T62

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T652

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T76

Suministrada por:

3 proveedores de Matmatch

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TD04

7000 Serie

AA Standards Grade 7075 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T651

Suministrada por:

3 proveedores de Matmatch

7000 Serie

EN 573-3 Grade 3.4365 T62

Suministrada por:

3 proveedores de Matmatch

Página 1 de 12