Acero inoxidable martensítico
ASTM A579 Grade 51 Type 3, Martensitic StainlessAcero inoxidable martensítico
ASTM A579 Grade 52 Type 3, Martensitic StainlessAcero inoxidable martensítico
ASTM A579 Grade 53 Type 3, Martensitic StainlessChromium Molybdenum Steel
ASTM A579 Grade 12 Type 1, Quench and TemperedNickel Chromium Molybdenum Steel
ASTM A579 Grade 21 Type 1, Quench and TemperedAcero inoxidable endurecido por precipitación
ASTM A579 Grade 64 Type 5, No. 2 Precipitation Hardening StainlessAcero inoxidable endurecido por precipitación
ASTM A579 Grade 61 Type 4, No. 1 Precipitation Hardening StainlessChromium Molybdenum Steel
ASTM A579 Grade 13 Type 1, Quench and TemperedNickel Chromium Molybdenum Steel
ASTM A579 Grade 22 Type 1, Quench and TemperedAcero inoxidable endurecido por precipitación
ASTM A579 Grade 62 Type 6, No. 3 Precipitation Hardening StainlessNickel Chromium Molybdenum Steel
ASTM A579 Grade 23 Type 1, Quench and Tempered