Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 35 J Show Material materials with Charpy impact energy of 35 J |
Elongation | 20.0 °C | 8 - 12 % Show Material materials with Elongation of 8 - 12 % |
Reduction of area | 20.0 °C | 40 - 50 % Show Material materials with Reduction of area of 40 - 50 % |
Tensile strength | 20.0 °C | 1140 - 1380 MPa Show Material materials with Tensile strength of 1140 - 1380 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.07 % Show Material materials with Carbon of 0.07 % |
Chromium | 15.5 - 17.5 % Show Material materials with Chromium of 15.5 - 17.5 % |
Copper | 3 - 5 % Show Material materials with Copper of 3 - 5 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 3 - 5 % Show Material materials with Nickel of 3 - 5 % |
Niobium | 0.15 - 0.45 % Show Material materials with Niobium of 0.15 - 0.45 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |