Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 20 J Show Material materials with Charpy impact energy of 20 J |
Elongation | 20.0 °C | 10 - 12 % Show Material materials with Elongation of 10 - 12 % |
Reduction of area | 20.0 °C | 25 % Show Material materials with Reduction of area of 25 % |
Tensile strength | 20.0 °C | 1140 - 1450 MPa Show Material materials with Tensile strength of 1140 - 1450 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.1 - 0.15 % Show Material materials with Carbon of 0.1 - 0.15 % |
Chromium | 15 - 16 % Show Material materials with Chromium of 15 - 16 % |
Manganese | 0.5 - 1.25 % Show Material materials with Manganese of 0.5 - 1.25 % |
Molybdenum | 2.5 - 3.25 % Show Material materials with Molybdenum of 2.5 - 3.25 % |
Nickel | 4 - 5 % Show Material materials with Nickel of 4 - 5 % |
Nitrogen | 0.07 - 0.13 % Show Material materials with Nitrogen of 0.07 - 0.13 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |