Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 15 - 45 J Show Material materials with Charpy impact energy of 15 - 45 J |
Elongation | 20.0 °C | 6 - 13 % Show Material materials with Elongation of 6 - 13 % |
Reduction of area | 20.0 °C | 25 - 40 % Show Material materials with Reduction of area of 25 - 40 % |
Tensile strength | 20.0 °C | 1035 - 1720 MPa Show Material materials with Tensile strength of 1035 - 1720 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1550 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.45 - 0.5 % Show Material materials with Carbon of 0.45 - 0.5 % |
Chromium | 0.9 - 1.2 % Show Material materials with Chromium of 0.9 - 1.2 % |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % |
Molybdenum | 0.9 - 1.1 % Show Material materials with Molybdenum of 0.9 - 1.1 % |
Nickel | 0.4 - 0.7 % Show Material materials with Nickel of 0.4 - 0.7 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.15 - 0.3 % Show Material materials with Silicon of 0.15 - 0.3 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Vanadium | 0.08 - 0.15 % Show Material materials with Vanadium of 0.08 - 0.15 % |