General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Density of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa | Typical for Martensitic Stainless Steel |
Elongation | 20.0 °C | 10 - 12 % Show Material materials with Elongation of 10 - 12 % | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Reduction of area | 20.0 °C | 40 - 45 % Show Material materials with Reduction of area of 40 - 45 % | |
Tensile strength | 20.0 °C | 1210 - 1520 MPa Show Material materials with Tensile strength of 1210 - 1520 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1100 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Thermal conductivity | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Thermal conductivity of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 6E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.2 - 0.25 % Show Material materials with Carbon of 0.2 - 0.25 % |
Chromium | 11 - 12.5 % Show Material materials with Chromium of 11 - 12.5 % |
Cobalt | 0.25 % Show Material materials with Cobalt of 0.25 % |
Manganese | 0.5 - 1 % Show Material materials with Manganese of 0.5 - 1 % |
Molybdenum | 0.9 - 1.25 % Show Material materials with Molybdenum of 0.9 - 1.25 % |
Nickel | 0.5 - 1 % Show Material materials with Nickel of 0.5 - 1 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Tin | 0.04 % Show Material materials with Tin of 0.04 % |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % |
Tungsten | 0.9 - 1.25 % Show Material materials with Tungsten of 0.9 - 1.25 % |
Vanadium | 0.2 - 0.3 % Show Material materials with Vanadium of 0.2 - 0.3 % |