2000 Serie
EN 573-3 Grade AW-2014 T62000 Serie
EN 573-3 Grade AW-2014 T62000 Serie
EN 573-3 Grade AW-2014 T6512000 Serie
EN 573-3 Grade AW-2014 T6516000 Serie
EN 573-3 Grade AW-6016 T6Acero bajo en carbono
EN 10216-2 Grade P195GH normalized or normalized formed (+N)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 quenched (+Q)Acero inoxidable austenítico
EN 10088-1 Grade X4CrNi18-12 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMo18-15-4 quenched (+Q)