Unclassified Low Alloy Steel
EN 10025-6 Grade S500Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Acero inoxidable austenítico
EN 10028-7 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1NiCrMoCuN25-20-7 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNiMoCuN25-25-5 solution annealed (+AT)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenched