Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
DIN 17155 Grade 10CrMo9-10 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10216-2 Grade 11CrMo9-10 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10222-2 Grade 11CrMo9-10 normalized and tempered (+NT)Chromium Molybdenum Steel
EN 10222-2 Grade 11CrMo9-10 quenched and tempered (+QT)Chromium Molybdenum Steel
ASTM A182 F22 Class 1 Annealed or Normalized and TemperedChromium Molybdenum Steel
ASTM A182 F22 Class 3 Annealed or Normalized and TemperedChromium Molybdenum Steel
ASTM A989 K21590 Class 1 Hot Isostatically-Pressed (HIP)Chromium Molybdenum Steel
EN 10273 Grade 11CrMo9-10 quenched and tempered (+QT)Chromium Molybdenum Steel
ASTM A336 F22 Class 1 Annealed or Normalized and TemperedChromium Molybdenum Steel
ASTM A336 F22 Class 3 Annealed or Normalized and TemperedChromium Molybdenum Steel
ASTM A213 Grade T22