Medidas
Property | Value |
---|---|
Diámetro | 20 - 353 mm Show Supplier Material materials with Diámetro of 20 - 353 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 260 [-] Show Supplier Material materials with Dureza Brinell of 260 [-] | soft annealed |
Dureza Rockwell C | 48 - 54 [-] Show Supplier Material materials with Dureza Rockwell C of 48 - 54 [-] | |
Resistencia a la tracción | 1555 - 1920 MPa Show Supplier Material materials with Resistencia a la tracción of 1555 - 1920 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered |
200 °C | 1.25e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.25e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered | |
300 °C | 1.3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.3e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered | |
Conductividad térmica | 100 °C | 27.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 27.7 W/(m·K) | |
150 °C | 28.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 28.9 W/(m·K) | ||
200 °C | 29.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 29.7 W/(m·K) | ||
250 °C | 30.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30.5 W/(m·K) | ||
300 °C | 31 W/(m·K) Show Supplier Material materials with Conductividad térmica of 31 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 1.4 % Show Supplier Material materials with Cromo of 1.4 % |
Hierro | Balance |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % |
Molibdeno | 0.2 % Show Supplier Material materials with Molibdeno of 0.2 % |
Níquel | 4 % Show Supplier Material materials with Níquel of 4 % |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutlery dies, cutting tools for thick materials, billet-shear blades, drawing jaws, massive embossing and bending tools, plastic moulds, reinforcements | |
Heat Treatment | Soft annealing: 610-650°C (Cooling in furnace) - Stress-relief-annealing: 600-650°C (cooling in Furnace), Hardening: 840-870°C and quenching in air, oil or salt bath: 180-220°C |