Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.48 % Show Supplier Material materials with Absorción de agua of 0.48 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.23 g/cm³ Show Supplier Material materials with Densidad of 1.23 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.16 % Show Supplier Material materials with Moisture absorption of 0.16 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore A | 98 [-] Show Supplier Material materials with Dureza Shore A of 98 [-] | dry | ISO 868 | 3s | |
98 [-] Show Supplier Material materials with Dureza Shore A of 98 [-] | dry | ISO 868 | 15s | ||
Dureza Shore D | 57.0 [-] Show Supplier Material materials with Dureza Shore D of 57.0 [-] | dry | ISO 868 | 3s | |
57.0 [-] Show Supplier Material materials with Dureza Shore D of 57.0 [-] | dry | ISO 868 | 15s | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.26 GPa Show Supplier Material materials with Módulo elástico of 0.26 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 148 kN/m Show Supplier Material materials with Resistencia a desgarros of 148 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 31 MPa Show Supplier Material materials with Resistencia a la tracción of 31 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 212 °C Show Supplier Material materials with Temperatura de fusión of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 110 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 110 °C | dry | ISO 306 | 50°C/h 50N |
200 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 200 °C | dry | ISO 306 | 50°C/h 10N | |
Temperatura de transición del vidrio | -30 °C Show Supplier Material materials with Temperatura de transición del vidrio of -30 °C | dry | ASTM D5026/D7028 | DMTA (E) |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|