General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.97 g/cm³ Show Supplier Material materials with Densidad of 1.97 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dureza Rockwell M | 101 [-] Show Supplier Material materials with Dureza Rockwell M of 101 [-] | dry | ISO 2039-2 | |
Elongación | -40 °C | 1 % Show Supplier Material materials with Elongación of 1 % | dry | ISO 527-1/-2 |
1 % Show Supplier Material materials with Elongación of 1 % | dry | ISO 527-1/-2 | ||
120 °C | 1.7 % Show Supplier Material materials with Elongación of 1.7 % | dry | ISO 527-1/-2 | |
160 °C | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | dry | ISO 527-1/-2 | |
180 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
200 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 230 MPa Show Supplier Material materials with Flexural yield strength of 230 MPa | dry | ISO 178 | |
120 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
160 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
200 °C | 85 MPa Show Supplier Material materials with Flexural yield strength of 85 MPa | dry | ISO 178 | |
Hardness, Rockwell R | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | dry | ISO 2039-2 | |
Módulo de flexión | 20 GPa Show Supplier Material materials with Módulo de flexión of 20 GPa | dry | ISO 178 | |
120 °C | 14 GPa Show Supplier Material materials with Módulo de flexión of 14 GPa | dry | ISO 178 | |
160 °C | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | dry | ISO 178 | |
200 °C | 7 GPa Show Supplier Material materials with Módulo de flexión of 7 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 23 GPa Show Supplier Material materials with Módulo elástico of 23 GPa | dry | ISO 527-1/-2 |
20 GPa Show Supplier Material materials with Módulo elástico of 20 GPa | dry | ISO 527-1/-2 | ||
120 °C | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | |
160 °C | 8.9 GPa Show Supplier Material materials with Módulo elástico of 8.9 GPa | dry | ISO 527-1/-2 | |
180 °C | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |
200 °C | 7.7 GPa Show Supplier Material materials with Módulo elástico of 7.7 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | dry | ISO 527-1/-2 |
145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | dry | ISO 527-1/-2 | ||
120 °C | 98 MPa Show Supplier Material materials with Resistencia a la tracción of 98 MPa | dry | ISO 527-1/-2 | |
160 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |
180 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
200 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6.8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.8 kJ/m² | dry | ISO 179/1eA |
23 °C | 6.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 27 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 27 kJ/m² | dry | ISO 179/1eU |
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 25 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-07 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | |||
2.7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
7.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.5e-07 1/K | dry | ISO 11359-1/-2 | normal, above Tg | |||
Conductividad térmica | 0.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.7 W/(m·K) | dry | ASTM E1461 | in plane | ||
0.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.7 W/(m·K) | dry | ASTM E1461 | through plane | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | UL746B | 0.7 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.7 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.7 mm | ||
Temperatura de flexión bajo carga | 230 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 230 °C | dry | ISO 75-1/-2 | 8 MPa | ||
277 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 277 °C | dry | ISO 75-1/-2 | 2 MPa | |||
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 90 °C Show Supplier Material materials with Temperatura de transición del vidrio of 90 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry | IEC 60250 | 1GHz |
5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | dry | IEC 60250 | 5GHz | |
Factor de disipación | 34 [-] Show Supplier Material materials with Factor de disipación of 34 [-] | dry | IEC 60250 | 1GHz |
44 [-] Show Supplier Material materials with Factor de disipación of 44 [-] | dry | IEC 60250 | 5GHz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 225 V Show Supplier Material materials with Índice de seguimiento comparativo of 225 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Crankshaft Covers, Coil insulation, Rectifier, Water pump part, Alternator bridges, Thermal management valve bodies | |
Fillers | 65% Glass Fiber and Mineral Powder |