General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.3 % Show Supplier Material materials with Elongación of 3.3 % | dry | ISO 527-1/-2 | |
Módulo de flexión | 13.6 GPa Show Supplier Material materials with Módulo de flexión of 13.6 GPa | dry | ISO 178 | |
Módulo elástico | 15.8 GPa Show Supplier Material materials with Módulo elástico of 15.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 167 MPa Show Supplier Material materials with Resistencia a la tracción of 167 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 20.1 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 20.1 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|
Difusividad térmica | 8.99e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 8.99e-08 mm²/s | dry | - | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 4800 Ω/sq Show Supplier Material materials with Surface resistivity of 4800 Ω/sq | conditioned | IEC 62631-3-2 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 1110 g/cm³ Show Supplier Material materials with Density of melt of 1110 g/cm³ | dry | - |
Specific heat capacity melt | 2830.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2830.0 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.28 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.28 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber and Carbon Fiber |