General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | dry | Sim. to ISO 62 |
Densidad | 1.54 g/cm³ Show Supplier Material materials with Densidad of 1.54 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | dry | ISO 527-1/-2 | |
Módulo elástico | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | dry | ISO 179/1eU |
23 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 215 °C Show Supplier Material materials with Ball pressure temperature of 215 °C | dry | IEC 60695-10-2 | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 2 mm | |||
Inflamabilidad | V-2 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 550 V Show Supplier Material materials with Índice de seguimiento comparativo of 550 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 250 °C | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Residual Current Breaker with Overload, Motor Starter/Overload Relays | |
Certifications | Yellow Card Available | |
Fillers | 25% Glass Fiber |