General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.45 % Show Supplier Material materials with Absorción de agua of 0.45 % | dry | Sim. to ISO 62 |
Densidad | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 250 °C | 75 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 75 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |